Brand Name: | TORICH |
Model Number: | ASTM B168 |
MOQ: | 1 TON |
Price: | 5000USD per ton |
Payment Terms: | T/T, L/C, D/A, D/P, Western Union, MoneyGram |
Supply Ability: | 5000 tons per year |
ASTM B168 Nickel Alloy Tube for Heat Exchanger
Application:
1) Evaporation tank, acid and alkali industrial machine in petrochemical production, catalytic regenerator,heat exchanger.
2) The production and use of corrosive alkali metals, especially in environments where sulfides are used,
3) Jet engine components, supplemental components of turbojet engines, etc.
Inconel 600 alloy is ni - cr - iron base alloy solid solution strengthening, has good resistance to high temperature corrosion and oxidation resistance, excellent hot and cold processing and welding performance, under 700 ℃ has a satisfactory heat intensity and high plasticity.Alloy can be strengthen through the cold work, also can use resistance welding, welding or soldering connection.
Physical properties | |||||
| -150℃ | 21℃ | 100℃ | 500℃ | 1000℃ |
Modulus of elasticity (Gpa) | 12.5 | | 15.9 | 22.1 | |
Mean coefficient of thermal expansion | | 210 | 210 | 187 | 143 |
Coefficient of heat conduction (w/m℃) | 10.9 | 10.4 | 13.3 | 14.9 | |
Specific heat capacity (j/kg.℃) | 310 | 444 | 465 | 536 | |
Than the resistance (Ωmm2/m) | | 1.03 | 1.04 | 1.12 | |
ASTM B168
Referenced ASTM Standard:
B166 Specification for Nickel-Chromium-Iron Alloy (UNS N06600, N06601, N06603, N06690, N06693, N06025, N06045, N06696),
Nickel-Chromium-Cobalt-Molybdeum Alloy (UNS N06617) and Nickel-Iron-Chromiun-Tungsten Alloy (UNS N06674) Rod, Bar and Wire.
B 880 Specification for general requirements for Chemical check analysis limits for Nickel, Nickel alloys and Cobalt alloys.
E 8 Test method for tension testing of metallic materials.
E10 Test method for brinell hardness of metallic material.
E 18 Test methods for rockwell hardness and rockwell superficial hardness od metallic materials.
E 29 Practice for using significant digits in test data to determine conformance with sprcifications.
E38 Methods for Chemical Analysis of Nickel-Chromium and Nickel-Chromium-Iron Alloy.
E 112 Test Methods for determining the average grain size.
E140 Hardness conversion tables for metal.
E527 Practice for numbering metals and alloys in the unified numbering system (UNS)
E 1473 Test methods for chemical analysis of Nickel, Cobalt and high-temperature alloys.
F155 Method of test for temper of strip and sheet metals for electronic devices (spring-Back method)
Keywords:
plate; sheet; strip; UNS N06025; UNS N06045; UNS N06600; UNS N06601; UNS N06603; UNS N06617; UNS N06674; UNS N06690; UNS N06693; UNS N06696