Oxidation Resistance Superalloy Inconel Pipe 0.299 lbs / in3 8.28 g / cm3 980℃

Basic Properties
Place of Origin: China
Brand Name: Torich
Certification: CE PED
Model Number: Inconel X-750
Trading Properties
Minimum Order Quantity: 1000kg
Price: 6000-20000 USD per ton
Payment Terms: L/C, T/T
Supply Ability: 200 tons per year
Product Summary
Inconel Steel Tue are produced with Inconel Alloy Steel Grade InconelX-750 Mechanical component C:≤0.08 Cr:14.0-17.0 Ni+Co:≥70.0 Al:0.40-1.00 Ti:2.25-2.75 Fe:5.00-9.00 Nb+Ta:0.70-1.20 Co:1.00max Mn:1.00max Si:0.50max S:0.010max Cu:0.50max P:0.015max Data for material physical properties: Desity : 0...

Product Details

Highlight:

inconel 600 tube

,

inconel 601 tube

Material: InconelX-750
Standard: AMS 5542,AMS 5598
Application: Industry
Grade: Alloy
Type: Nickel Pipe
Product Description

Inconel Steel Tue are produced with Inconel Alloy Steel Grade InconelX-750

 

 

Mechanical component

C:≤0.08

Cr:14.0-17.0

Ni+Co:≥70.0

Al:0.40-1.00

Ti:2.25-2.75

Fe:5.00-9.00

Nb+Ta:0.70-1.20

Co:1.00max

Mn:1.00max

Si:0.50max

S:0.010max

Cu:0.50max

P:0.015max

 

Data for material physical properties:

 

Desity : 0.299lbs/in3,8.28g/cm3

 

InconelX-750 thermal conductivity

θ/℃ 50 100 300 500 900

λ/(W/(m·℃))

14.7 15.9 20.1 25.1 37.3

 

InconelX-750 line expansion coefficient

θ/℃ 20~200 20~300 20~400 20~500 20~600 20~700 20~800
α/10-6℃-1 13.1 13.5 14.1 14.4 15.0 15.6 16.2

 

Characteristic:

InconelX-750 alloy Nickel-base superalloy.

 

Below 980℃ with good resistance ro corrosion and oxidation resistance

Below  800℃ has higher strength 

Below 540℃ has good resistance to relaxation properties, good formability and weldability as well.

 

Application is aircraft engines.

 

Heat treatment process:

Annealing 955-1010℃,water-cooled

Weldment before welding annealing 980℃,1h

weldement stress relief annealing900℃ moisture 2h

Stress relief annealing 885℃,±15℃,24h,air cooling.

 

InconelX-750 mechanical properties.

 

σb/MPa≤965

σP0.2/MPa≤550

δ4D/%≥35

 

 with the condition of 980 ℃ ± 15 ℃, holding the appropriate time, air cooling or rapid cooling, descaling.

 

σb/MPa≥1170

σP0.2/MPa≥790

δ4D/%≥15

 

with the condition of+ 730 ℃ ± 10 ℃, 8h, furnace cooling 55 ℃ / h or air cooling to 620 ℃ ± 10 ℃, 8h, air-cooled, the total aging time is not less than 18h

 

Related standard:AMS 5542,AMS 5598

 

Application for engine part.

 

Oxidation Resistance Superalloy Inconel Pipe 0.299 lbs / in3 8.28 g / cm3 980℃

 

Related Products
  • Auto Parts ASTM A513 Cold Rolling Welded Steel Tubes with DOM Production

    Auto Parts ASTM A513 Welded Steel Tubes with DOM production ASTM A513 Electric-Resistance-Welded Carbon and Alloy Steel Mechanical Tubing Applications: for Machinery, Mechanical Engineering 1. Standard: ASTM A513 cold rolling welded precision steel tubes 2. Steel Grade: SAE1010, SAE1020, other ...
  • 25mm Diameter Bright Annealing Seamless Steel Tube for Hydraulic Systems

    EN10305-1 E235 E355 NBK Bright Annealing Precision Steel Pipes for Hydraulic Systems EN10305-1 NBK Bright Annealed Precision steel pipes for Hydraulic system OD:4-80 (mm) WT0.5-10 (mm) Length 1000-12000mm Product name: Seamless Precision Steel Pipe Application: for hydraulic systems precision steel ...
  • Precision Seamless Black Phosphating Steel Tube for Hydraulic Systems

    Steel Pipes with high precision for Hydraulic Systems with Black Phosphating surface Black Phosphated Hydraulic Tubes with High Precision and tight tolerance, the tubes are produced by precision cold drawn and cold rolling, then bright annealed in a protected atmosphere, afterwards it is blackphosph...
  • Precision Seamless Galvanized Steel Tubes DIN2391 EN103052 ST35.0 ST37

    Precision Seamless Galvanized Steel Tubes DIN2391 EN103052 ST35.0 ST37 Production Process: Cold rolling by Cold pilger machine and Cold rolling machine,galvanized and zinc plated could be applied. Cold Rolled and Galvanized Steel Tube Production process: DIN highly accurate, cold rolled and bright ...

Send An Inquiry