| MOQ: | 1Ton |
| Price: | Negotiable |
| Standard Packaging: | In bundles or in wooden boxes. |
| Delivery Period: | 20-40days |
| Payment Method: | L/C,D/A,D/P,T/T,Western Union, |
| Supply Capacity: | 60000 Ton/Tons per Year |
| Item | Specification |
|---|---|
| Material | Low carbon steel / low alloy heat-resistant steel |
| Standard | TU 14-3-460 / TU 14-3-460-2003 / TU 14-3-460-2009 |
| Main Grades | 20, 20-PV, 15GS, 15ChM / 15CrMo, 12Ch1MF / 12Cr1MoV, 15H1M1F |
| Outside Diameter | Cold-formed: 10-76 mm; hot-formed: 57-219 mm |
| Wall Thickness | Cold-formed: 2-12 mm; hot-formed: 3.5-40 mm |
| Length | 1-12 m, customizable; TU 14-3-460-75 commonly lists length up to 9 m by agreement |
| OD Tolerance | Hot-rolled 57-219 mm: ±1%; cold-drawn 10-30 mm: ±0.30 mm; 32-50 mm: ±0.40 mm; 51-76 mm: ±0.8% |
| Wall Thickness Tolerance | Hot-rolled OD ≤108 mm: +15% / -10%; OD >108 mm: +20% / -5%; cold-drawn 2-12 mm: ±10% |
| Straightness | Controlled for boiler installation and tube-bank assembly; tighter straightness available by agreement |
| Surface Condition | Pickled, shot-blasted, polished, oiled, or as-heat-treated |
| Heat Treatment | Normalizing; normalizing + tempering for alloy heat-resistant grades |
| Inspection | 100% non-destructive testing, dimensional inspection, hydrostatic or equivalent testing by order requirement |
| Feature | Technical Value |
|---|---|
| High-pressure boiler service | Designed for steam boilers and pipelines with high and supercritical steam parameters |
| Seamless structure | No weld seam, suitable for pressure-bearing boiler circuits |
| Wide size coverage | Cold-formed 10-76 mm OD; hot-formed 57-219 mm OD |
| Heat-resistant alloy options | 12Ch1MF / 12Cr1MoV contains Cr 0.90-1.20%, Mo 0.25-0.35%, V 0.15-0.30% |
| Strength range | 20 / 20-PV: 412-549 MPa tensile strength; 12Cr1MoV and 15CrMo: 441-637 MPa tensile strength |
| Ductility control | Minimum elongation commonly 21-24% for 20-PV, 15CrMo, and 12Cr1MoV grades |
| NDT requirement | TU 14-3-460-75 product references specify 100% non-destructive testing |
| Buyer Concern | Our Solution |
|---|---|
| Grade selection for temperature and pressure | We help match 20-PV, 15GS, 15CrMo, 12Cr1MoV, or 15H1M1F according to boiler zone, steam temperature, wall thickness, and creep-resistance requirement. |
| Dimensional risk during boiler assembly | We control OD, wall thickness, ovality, straightness, and cut length according to TU 14-3-460 tolerance logic, with additional agreement available for tube-bank fabrication. |
| Material traceability and inspection reliability | Each batch can be supplied with heat number tracking, chemical analysis, mechanical test report, heat-treatment record, NDT record, and EN 10204 3.1-type inspection documentation when required. |
| Standard System | Related Standard / Equivalent Direction |
|---|---|
| GOST / TU | TU 14-3-460, TU 14-3R-55, GOST-related boiler tube specifications |
| ASTM / ASME | ASTM A192, ASTM A210, ASTM A213, ASTM A335, ASME SA213 / SA335 depending on grade equivalence |
| EN | EN 10216-2 for seamless pressure tubes; P235GH, 16Mo3, 13CrMo4-5, 10CrMo9-10 as project-based alternatives |
| JIS | JIS G3461, JIS G3462 for boiler and heat exchanger tubes |
| GB | GB 3087, GB/T 5310 for medium and high-pressure boiler tubes |
| Grade | C % | Si % | Mn % | P % max | S % max | Cr % | Ni % | Cu % | Mo % | V % | Fe |
|---|---|---|---|---|---|---|---|---|---|---|---|
| 20 / 20-PV | 0.17-0.24 | 0.17-0.37 | 0.35-0.65 | 0.025-0.030 max | 0.030 max | 0.25 max | 0.25 max | 0.30 max | -- | -- | Balance |
| 15GS | 0.12-0.18 | 0.70-1.00 | 0.90-1.30 | 0.025 max | 0.025 max | 0.30 max | 0.30 max | 0.30 max | -- | -- | Balance |
| 15ChM / 15CrMo | 0.11-0.18 | 0.17-0.37 | 0.40-0.70 | 0.025 max | 0.025 max | 0.80-1.10 | 0.30 max | 0.30 max | 0.40-0.55 | -- | Balance |
| 12Ch1MF / 12Cr1MoV | 0.10-0.15 | 0.17-0.37 | 0.40-0.70 | 0.025 max | 0.025 max | 0.90-1.20 | 0.25 max | 0.20 max | 0.25-0.35 | 0.15-0.30 | Balance |
| 15H1M1F | 0.10-0.15 | 0.17-0.37 | 0.40-0.70 | 0.025 max | 0.025 max | 1.10-1.40 | 0.25 max | 0.25 max | 0.90-1.10 | 0.20-0.35 | Balance |
| Grade | Heat Treatment / Delivery Condition | Tensile Strength, MPa | Yield Strength, MPa | Elongation, % min | Notes |
|---|---|---|---|---|---|
| 20 / 20-PV | Normalized or as specified | 412-549 | 216 min | 24 longitudinal / 22 transverse | Carbon boiler tube grade |
| 15GS | Normalized 900-930°C, air cooling | 490-640 | 295 min | 16-18 min | Si-Mn low alloy boiler tube grade |
| 15ChM / 15CrMo | Normalized + tempering as required | 441-637 | 235 min | 21 longitudinal / 20 transverse | Cr-Mo heat-resistant grade |
| 12Ch1MF / 12Cr1MoV | Normalized + tempering as required | 441-637 | 274 min | 21 longitudinal / 19 transverse | Cr-Mo-V heat-resistant grade |
| 15H1M1F | Normalized 970-1000°C + tempered 730-760°C | 490-690 | 345 min | 16-18 min | Higher Mo-V heat-resistant grade |
| MOQ: | 1Ton |
| Price: | Negotiable |
| Standard Packaging: | In bundles or in wooden boxes. |
| Delivery Period: | 20-40days |
| Payment Method: | L/C,D/A,D/P,T/T,Western Union, |
| Supply Capacity: | 60000 Ton/Tons per Year |
| Item | Specification |
|---|---|
| Material | Low carbon steel / low alloy heat-resistant steel |
| Standard | TU 14-3-460 / TU 14-3-460-2003 / TU 14-3-460-2009 |
| Main Grades | 20, 20-PV, 15GS, 15ChM / 15CrMo, 12Ch1MF / 12Cr1MoV, 15H1M1F |
| Outside Diameter | Cold-formed: 10-76 mm; hot-formed: 57-219 mm |
| Wall Thickness | Cold-formed: 2-12 mm; hot-formed: 3.5-40 mm |
| Length | 1-12 m, customizable; TU 14-3-460-75 commonly lists length up to 9 m by agreement |
| OD Tolerance | Hot-rolled 57-219 mm: ±1%; cold-drawn 10-30 mm: ±0.30 mm; 32-50 mm: ±0.40 mm; 51-76 mm: ±0.8% |
| Wall Thickness Tolerance | Hot-rolled OD ≤108 mm: +15% / -10%; OD >108 mm: +20% / -5%; cold-drawn 2-12 mm: ±10% |
| Straightness | Controlled for boiler installation and tube-bank assembly; tighter straightness available by agreement |
| Surface Condition | Pickled, shot-blasted, polished, oiled, or as-heat-treated |
| Heat Treatment | Normalizing; normalizing + tempering for alloy heat-resistant grades |
| Inspection | 100% non-destructive testing, dimensional inspection, hydrostatic or equivalent testing by order requirement |
| Feature | Technical Value |
|---|---|
| High-pressure boiler service | Designed for steam boilers and pipelines with high and supercritical steam parameters |
| Seamless structure | No weld seam, suitable for pressure-bearing boiler circuits |
| Wide size coverage | Cold-formed 10-76 mm OD; hot-formed 57-219 mm OD |
| Heat-resistant alloy options | 12Ch1MF / 12Cr1MoV contains Cr 0.90-1.20%, Mo 0.25-0.35%, V 0.15-0.30% |
| Strength range | 20 / 20-PV: 412-549 MPa tensile strength; 12Cr1MoV and 15CrMo: 441-637 MPa tensile strength |
| Ductility control | Minimum elongation commonly 21-24% for 20-PV, 15CrMo, and 12Cr1MoV grades |
| NDT requirement | TU 14-3-460-75 product references specify 100% non-destructive testing |
| Buyer Concern | Our Solution |
|---|---|
| Grade selection for temperature and pressure | We help match 20-PV, 15GS, 15CrMo, 12Cr1MoV, or 15H1M1F according to boiler zone, steam temperature, wall thickness, and creep-resistance requirement. |
| Dimensional risk during boiler assembly | We control OD, wall thickness, ovality, straightness, and cut length according to TU 14-3-460 tolerance logic, with additional agreement available for tube-bank fabrication. |
| Material traceability and inspection reliability | Each batch can be supplied with heat number tracking, chemical analysis, mechanical test report, heat-treatment record, NDT record, and EN 10204 3.1-type inspection documentation when required. |
| Standard System | Related Standard / Equivalent Direction |
|---|---|
| GOST / TU | TU 14-3-460, TU 14-3R-55, GOST-related boiler tube specifications |
| ASTM / ASME | ASTM A192, ASTM A210, ASTM A213, ASTM A335, ASME SA213 / SA335 depending on grade equivalence |
| EN | EN 10216-2 for seamless pressure tubes; P235GH, 16Mo3, 13CrMo4-5, 10CrMo9-10 as project-based alternatives |
| JIS | JIS G3461, JIS G3462 for boiler and heat exchanger tubes |
| GB | GB 3087, GB/T 5310 for medium and high-pressure boiler tubes |
| Grade | C % | Si % | Mn % | P % max | S % max | Cr % | Ni % | Cu % | Mo % | V % | Fe |
|---|---|---|---|---|---|---|---|---|---|---|---|
| 20 / 20-PV | 0.17-0.24 | 0.17-0.37 | 0.35-0.65 | 0.025-0.030 max | 0.030 max | 0.25 max | 0.25 max | 0.30 max | -- | -- | Balance |
| 15GS | 0.12-0.18 | 0.70-1.00 | 0.90-1.30 | 0.025 max | 0.025 max | 0.30 max | 0.30 max | 0.30 max | -- | -- | Balance |
| 15ChM / 15CrMo | 0.11-0.18 | 0.17-0.37 | 0.40-0.70 | 0.025 max | 0.025 max | 0.80-1.10 | 0.30 max | 0.30 max | 0.40-0.55 | -- | Balance |
| 12Ch1MF / 12Cr1MoV | 0.10-0.15 | 0.17-0.37 | 0.40-0.70 | 0.025 max | 0.025 max | 0.90-1.20 | 0.25 max | 0.20 max | 0.25-0.35 | 0.15-0.30 | Balance |
| 15H1M1F | 0.10-0.15 | 0.17-0.37 | 0.40-0.70 | 0.025 max | 0.025 max | 1.10-1.40 | 0.25 max | 0.25 max | 0.90-1.10 | 0.20-0.35 | Balance |
| Grade | Heat Treatment / Delivery Condition | Tensile Strength, MPa | Yield Strength, MPa | Elongation, % min | Notes |
|---|---|---|---|---|---|
| 20 / 20-PV | Normalized or as specified | 412-549 | 216 min | 24 longitudinal / 22 transverse | Carbon boiler tube grade |
| 15GS | Normalized 900-930°C, air cooling | 490-640 | 295 min | 16-18 min | Si-Mn low alloy boiler tube grade |
| 15ChM / 15CrMo | Normalized + tempering as required | 441-637 | 235 min | 21 longitudinal / 20 transverse | Cr-Mo heat-resistant grade |
| 12Ch1MF / 12Cr1MoV | Normalized + tempering as required | 441-637 | 274 min | 21 longitudinal / 19 transverse | Cr-Mo-V heat-resistant grade |
| 15H1M1F | Normalized 970-1000°C + tempered 730-760°C | 490-690 | 345 min | 16-18 min | Higher Mo-V heat-resistant grade |