Aircraft Engine Hastelloy X Alloy Steel Pipe Nickel Based Superalloy With Iron

Aircraft Engine Hastelloy X Alloy Steel Pipe Nickel Based Superalloy With Iron

alloy steel seamless tube

seamless alloy steel pipe

Place of Origin:

China

Brand Name:

Torich

Certification:

CE PED

Model Number:

Alloy Steel Pipe HastelloyX

Contact Us
Request A Quote
Product Details
Similar Grade:
GH3536, GH536,GH22, GH334, GH739, SG-5, UNS N06002, NC22FeD, NiCr22FeMo, Nimonic PE13
Material:
Hastelloy C
Application:
Used In The Manufacture Of Aircraft Engine Combustion Chamber Components And Other High Temperature Components
Density:
8.28g/cm³
Melting Temperature:
1295℃-1381℃
Highlight:

alloy steel seamless tube

,

seamless alloy steel pipe

Payment & Shipping Terms
Minimum Order Quantity
1000kg
Price
negotiable
Packaging Details
In bundles in woode box
Delivery Time
6-8 weeks
Payment Terms
L/C, T/T
Supply Ability
200 tons per year
Product Description

Alloy Steel Pipe HastelloyX

 

Hastelloy X is a kind of nickel-based superalloy with high iron content, which is mainly solution strengthened by chromium and molybdenum solution strengthening. It has good resistance to oxidation and corrosion resistance. It has good cold & hot formability and weldability because its moderate lasting and creep strength under 900℃. Used in the manufacture of aircraft engine combustion chamber components and other high temperature components. It can be long-term used under 900℃, and short-term working temperature can up to 1080℃.

 

Similar Grade of Hastelloy X:  GH3536, GH536,GH22, GH334, GH739, SG-5, UNS N06002, NC22FeD, NiCr22FeMo, Nimonic PE13, Hastelloy H

 

Application for Hastelloy X: Used in the manufacture of aircraft engine combustion chamber components and other high temperature components

 

Chemical Composition of Hastelloy X:

 

Chemical Composition (%)
C Cr Ni Co W Mo Al Ti Fe B Cu Mn Si P S
0.05-0.15 20.5-23.0 Margin 0.50-2.50 0.20-1.00

8.0-

10.0

≤0.50 ≤0.15 17.0-20.0 ≤0.010 ≤0.5 ≤1.00 ≤1.00 ≤0.025 ≤0.015

 

Hastelloy X Physical Properties:

 

Hastelloy X Density: ρ: 8.28g/cm³

 

Hastelloy X Melting Temperature Rage: 1295℃-1381℃

 

Coefficient of Thermal Conductivity of Hastelloy X:

 

coefficient of thermal conductivity
Temperature
100 200 300 400 500 600 700 800 900
λ/(w/(m.℃)) 13.38 17.97 20.27 22.4 24.62 26.79 29.05 31.14

33.44

 

Specific Heat Capacity for Hastelloy X:

 

Specific Heat Capacity
Temperature
17 100 200 300 400 500 600 700 800 900
C/J/( kg · K ) 372.6 372.6 389.4 456.4 427.1 452.2 464.7 515 535.9 561

 

Expansion Coefficient for Hastelloy X:

 

expansion coefficient
Temperature/℃ 20-100 20-200 20-300 20-400 20-500 20-600 20-700 20-800 20-900
α1/10-6℃-1 12.1 12.5 13.4 14 14.3 14.8 15.5 15.8 16.1

 

Resistivity of Hastelloy X:

 

resistivity
Temperature/℃ 100 200 300 400 500 600 700 800 900
Resistor
Ω·m
1.18 1.2 1.21 1.22 1.24 1.25 1.26 1.27 1.29

 

 

Hastelloy X is widely used in aircraft engine and the civilian industry in adroad, and in our country, it mainly used in the manufacture of hot end of combustion chamber parts and other components, and honeycomb structure, etc. Besides, long-term used at high temperature will have certain age hardening phenomenon.

 

Aircraft Engine Hastelloy X Alloy Steel Pipe Nickel Based Superalloy With Iron 0 Aircraft Engine Hastelloy X Alloy Steel Pipe Nickel Based Superalloy With Iron 1

Send your inquiry directly to us

Privacy Policy China Good Quality Precision Steel Tube Supplier. Copyright © 2015-2025 TORICH INTERNATIONAL LIMITED . All Rights Reserved.