304 316 Welded Austenitic Stainless Steel Tube For Boilers / Heat Exchanger

Minimum Order Quantity : 1000kgs Price : negotiable
Packaging Details : In bundles or Wooden box Delivery Time : 4-6 weeks
Payment Terms : L/C, T/T Supply Ability : 50000 tons per year
Place of Origin: China Brand Name: TORICH
Certification: ISO 9001:2008, ISO 14001:2008, TS16949, CE, PED Model Number: ASTM A249

Detail Information

Material: Stainless Steel Type: Welded Stainless Steel
Application: Boilers, Superheater, Heat-Exchanger, Condenser Size: Up To 127mm OD
High Light:

stainless steel round tube

,

stainless tube steel

Product Description

ASTM A249 304 316 Welded Austenitic Stainless Steel Tube for Boilers / Heat Exchanger

 

 

Size:  

OD:  1/8 in (3.2mm) to 5 in (127mm)

WT:   0.015 to 0.320 in  (0.4 to 8.1mm)

 

Grade:

TP304H, TP309H, TP310H, TP316H, TP312H, TP347H and TP348H.

TP304, TP309S, TP310S, TP310Cb, TP316, TP321, TP347, TP348

For high-temperature service such as for superheaters and reheaters

 

Application:

Boiler, Superheater, Heat Exchanger, Condensor Tubes

Austenitic stainless steel, temperature service applications, high temperature applications

 

Manufacture:

The tubes are made from flat-rolled steel by an automatic welding process with no addition of filler metal.

Subsequent to welding and prior to final heat treatment, the tubes are cold worked on weld and base metal or in weld metal

 

Test and inspection:

Tension test

Flattening test

Flange test

Reverse-Bend test

Hardness test

Hydrostatic or Nondestructive Electric Test

Grain size

 

Table 1 Chemical Composition(cast analysis)a of Austenitic Corrosion Resisting Steels,in % By Mass(continued)

Steel Grade

C

max

Si Mn

P

max

S

max

N Cr Cu Mo Nb Ni Ti Others
Steel Name Steel Number
X2CrNi18-9 1.4307 0.030 ≤1.00 ≤2.00 0.040 0.015b ≤0.11 17.50 to 19.50 - - - 8.00 to 10.00c - -
X2CrNi19-11 1.4306 0.030 ≤1.00 ≤2.00 0.040 0.015b ≤0.11 18.00 to 20.00 - - - 10.00 to 12.00d - -
X2CrNiN18-10 1.4311 0.030 ≤1.00 ≤2.00 0.040 0.015 0.12-0.22 17.00 to 19.50 - - - 8.50 to 11.50 - -
X5CrNi18-10 1.4301 0.07 ≤1.00 ≤2.00 0.040 0.015 b ≤0.11 17.00 to 19.50 - - - 8.00 to 10.50 - -

X6CrNiTi18

-10

1.4541 0.08 ≤1.00 ≤2.00 0.040 0.015 - 17.00 to 19.00 - - - 9.00 to 12.00d

5xC

to

0.70

-

X6CrNiNb18

-10

1.4550 0.08 ≤1.00 ≤2.00 0.040 0.015 - 17.00 to 19.00 - -

10xC

to

1.00

9.00 to 12.00d - -
X1CrNi25-21 1.4335 0.020 ≤0.25 ≤2.00 0.025 0.010 ≤0.11 24.00 to 26.00 - ≤0.20 - 20.00 to 22.00 - -
X2CrNiMo17-12-2 1.4404 0.030 ≤1.00 ≤2.00 0.040 0.015 b ≤0.11 16.50 to 18.50 -

2.00to

2.50

- 10.00 to 13.00e - -
X5CrNiMo17-12-2 1.4401 0.07 ≤1.00 ≤2.00 0.040 0.015 b ≤0.11 16.50 to 18.50 -

2.00to

2.50

- 10.00 to 13.00 - -

X1CrNiMoN

25-22-2

1.4466 0.020 ≤0.70 ≤2.00 0.025 0.010

0.10to

0.16

24.00 to 26.00 -

2.00to

2.50

- 21.00 to 23.00 - -

X6CrNiMoTi

17-12-2

1.4571 0.08 ≤1.00 ≤2.00 0.040 0.015 b - 16.50 to 18.50 -

2.00to

2.50

- 10.50 to 13.50c

5xC

to

0.70

-

X6CrNiMoNb

17-12-2

1.4580 0.08 ≤1.00 ≤2.00 0.040 0.015 - 16.50 to 18.50 -

2.00to

2.50

10xC-1.00 10.50 to 13.50 - -

X2CrNiMoN

17-13-3

1.4429 0.030 ≤1.00 ≤2.00 0.040 0.015

0.12to

0.22

16.50 to 18.50 -

2.00to

3.00

- 11.00 to 14.00d - -

X3CrNiMo17

-13-3

1.4436 0.05 ≤1.00 ≤2.00 0.040 0.015 b ≤0.11 16.50 to 18.50 -

2.00to

3.00

- 10.50 to 13.00d - -
X2CrNiMo18-14-3 1.4435 0.030 ≤1.00 ≤2.00 0.040 0.015 b ≤0.11 17.00 to 19.00 -

2.00to

3.00

- 12.50 to 15.00 - -

X2CrNiMoN17

-13-5

1.4439 0.030 ≤1.00 ≤2.00 0.040 0.015

0.12to

0.22

16.50 to 18.50 -

4.00to

5.00

- 12.50 to 14.50 - -
Steel Grade

C

max

Si Mn

P

max

S

max

N Cr Cu Mo Nb Ni Ti Others
Steel name Steel name

X1NiCrMoCu

31-27-4

1.4563 0.020 ≤0.70 ≤2.00 0.030 0.010 ≤0.11 26.00 to 28.00

0.70

to

1.50

3.00

to

4.00

-

30.00

to

32.00

- -

X1NiCrMoCu

25-20-5

1.4539 0.020 ≤0.70 ≤2.00 0.030 0.010 ≤0.15 19.00 to 21.00

1.20

to

2.00

4.00

to

5.00

-

24.00

to

26.00

- -

X1CrNiMoCuN

20-18-7

1.4547 0.020 ≤0.70 ≤1.00 0.030 0.010

0.18to

0.25

19.50 to 20.50

0.50

to

1.00

6.00

to

7.00

-

17.50

to

18.50

- -

X1NiCrMoCuN

25-20-7

1.4529 0.020 ≤0.50 ≤1.00 0.030 0.010

0.15to

0.25

19.00 to 21.00

0.50

to

1.50

6.00

to

7.00

-

24.00

to

26.00

- -
X2NiCrAlTi32-20 1.4558 0.030 ≤0.70 ≤1.00 0.020 0.015 - 20.00 to 23.00 - - -

32.00

to

35.00

8x(C+N)

to0.60

Al:0.15

To0.45

  1. Elements not listed in this table shall not be intentionally added to the steel without the agreement of the purchaser except for finishing the cast.All appropriate precautions are to be taken to avoid the addition of such elements from scrap and other materials used in production which would impair mechanical properties and the suitability of the steel.
  2. For products to be machined a controlled sulphur content of 0.015% to 0.030% is permitted by agreement provided the resistance to corrosion is still satisfied for the intended purpose.

Option3:A sulphur content of 0.015% to 0.030% is specified.

  1. Where for special reasons,e.g. hot workability it is necessary to minimize the deltaferrite content,or with the aim of low permeability,the maximum nickel content may be increased by 0.50%
  2. Where for special reasons,e.g. hot workability it is necessary to minimize the deltaferrite content,or with the aim of low permeability,the maximum nickel content may be increased by 1.00%
  3. Where for special reasons,e.g. hot workability it is necessary to minimize the deltaferrite content,or with the aim of low permeability,the maximum nickel content may be increased by 1.50%

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

304 316 Welded Austenitic Stainless Steel Tube For Boilers / Heat Exchanger 0  304 316 Welded Austenitic Stainless Steel Tube For Boilers / Heat Exchanger 1

304 316 Welded Austenitic Stainless Steel Tube For Boilers / Heat Exchanger 2

 

 

 

 

SUPPLEMENTARY REQUIREMENTS

S1 - Stress-Relieved Annealed Tubes

S2 - Minimum Wall Tubes

S3- Air Underwater Pressure Test

S4 - Stabilizing Heat Treatment

S5 - Unstraightened Tubes

S6 - Intergranular Corrosion Test

S7 - Weld Decay Test

S8 - Special Applications

S9 - Additional Tesing of Welding Tubing per ASME Request

 

Referenced Documents:

ASTM Standards:

ASTM A262     Practices for Detecting Susceptibility to Intergranular Attack in Austenitic Stainless Steels

 

ASTM A480/ A480M   Specification for General Requirements for Flat-Rolled Stainless and Heat-Resisting Steel Plate, Sheet, and Strip

 

ASTM A1016/ A1016M  Specification for General Requirements for Ferritic Alloy Steel, Austenitic Alloy Steel, and Stainless Steel Tubes

 

E 112    Test Methods for Determining Average Grain Size

 

E213     Practice for Ultrasonic Examination of Metal Pipe and Tubing

 

E273     Practice for Ultrasonic Examination of Weld Zone of Welded Pipe and Tubing

 

E527     Practice for Numbering Metals and Alloys (UNS)

You Might Be Into These
Get in touch with us

Enter Your Message

sales3@steel-tubes.com
+8613736164628
+8613736164628
torichinternational
+86-13736164628
torichinternational@yahoo.com
174524687
174524687
+86-13736164628