ASTM A511 TP316 304 Thick Wall Seamless Stainless Steel Pipe For Mechanical
Contact Person : Richard SHEN
Phone Number : +86-13736164628
WhatsApp : +8613736164628
Minimum Order Quantity : | 5MT | Price : | negotiable |
---|---|---|---|
Packaging Details : | In bundles or wooden boxes | Delivery Time : | 30~45days |
Payment Terms : | L/C, T/T | Supply Ability : | 6000MT/Month |
Place of Origin: | China | Brand Name: | Torich |
---|---|---|---|
Certification: | ISO 9001:2008 , TS16949 , KR , RINA | Model Number: | ASTM A688 |
Detail Information |
|||
Dimension:: | OD 230mm WT≥0.7mm | Section Shape:: | Round |
---|---|---|---|
Product Name:: | Stainless Steel Tube | Grade:: | TP304/304L/304LN , TP316/316L/316LN |
High Light: | stainless steel round tube,large diameter stainless steel tube |
Product Description
ASTM A688 TP304/304L/304LN , TP316/316L/316LN Welded Austenitic Stainless Steel Feed warter Heater Tubes
Size range:
O.D.: 4.0-230mm W.T.:1-30mm L: according to customer requirement
Material and Manufacture:
Tubes are made from Flat-rolled steel by automatic welding process.
Subsequent to welding and prior to final heat treatment, the tubes are cold drawn or cold rolled
The tubes are ready for U-bending after annealed, according to customer's drawing and design.
Surface Condition:
The tubes are pickled in nitric and hydrofluoric acids.
Bright annealing.
Mechanical Requirement
Grade: |
TP304 |
TP304L |
TP304LN |
TP316 |
TP316L |
TP316LN |
TP316LN |
TPXM-29 |
TP304N |
UNS |
S30400 |
S30403 |
S30453 |
S31600 |
S31603 |
S31653 |
S31653 |
S24000 |
S30451 |
C, max |
0.08 |
0.035 |
0.035 |
0.080 |
0.035 |
0.035 |
0.035 |
0.08 |
0.080 |
Mn, max |
2.00 |
2.00 |
2.00 |
2.00 |
2.00 |
2.00 |
2.00 |
11.5-14.5 |
2.00 |
P, max |
0.045 |
0.045 |
0.045 |
0.045 |
0.045 |
0.045 |
0.045 |
0.060 |
0.045 |
S, max |
0.030 |
0.030 |
0.030 |
0.030 |
0.030 |
0.030 |
0.030 |
0.030 |
0.030 |
Si, max |
1.00 |
1.00 |
1.00 |
1.00 |
1.00 |
1.00 |
1.00 |
1.00 |
1.00 |
Ni |
18.0-20.0 |
18.0-20.0 |
18.0-20.0 |
16.0-18.0 |
16.0-18.0 |
16.0-18.0 |
16.0-18.0 |
17.0-19.0 |
18.0-20.0 |
Cr |
8.0-11.0 |
8.0-13.0 |
8.0-12.0 |
11.0-14.0 |
10.0-14.0 |
11.0-14.0 |
11.0-14.0 |
2.3-3.7 |
8.0-18.0 |
Mo |
… |
… |
… |
2.00-3.00 |
2.00-3.00 |
2.00-3.00 |
2.00-3.00 |
… |
… |
Nitrogen |
… |
… |
… |
… |
… |
… |
… |
… |
… |
Copper |
… |
… |
… |
… |
… |
|
|
|
|
Grade: | TP316N | … | … | … | … |
UNS | S31651 | N08367 | N08926 | S31254 | S32654 |
C, max | 0.070 | 0.030 | 0.020 | 0.020 | 0.020 |
Mn, max | 2.00 | 2.00 | 2.00 | 1.00 | 2.0-4.0 |
P, max | 0.045 | 0.040 | 0.030 | 0.030 | 0.030 |
S, max | 0.030 | 0.030 | 0.010 | 0.100 | 0.005 |
Si, max | 4.8-6.0 | 1.00 | 0.50 | 0.80 | 0.50 |
Ni | 9.58.0 | 20.0-22.0 | 24.0-26.0 | 19.5-20.5 | 21.0-23.0 |
Cr | 19.0-22.0 | 23.5-25.5 | 19.0-21.0 | 17.5-18.5 | 24.0-25.0 |
Mo | 0.30-1.50 | 6.0-7.0 | 6.0-7.0 | 6.0-6.5 | 7.0-8.0 |
Nitrogen | … | … | … | … | 0.45-0.55 |
Copper | … | … | … | 0.30-0.60 |
Tensil Requirements
Grade and UNS | Tensile strength min ksi [Mpa] |
Yield strength min ksi [Mpa] |
Elongation in 2in or 50mm min % |
||||||
304, 316 S30400, S31600 |
75 [515] | 30 [205] | 35 | ||||||
304L, 316L S30403, S31603 |
70 [485] | 25 [175] | 35 | ||||||
XM-29 S24000 |
100 [690] | 55 [380] | 35 | ||||||
304N, 316N S30451, S31651 |
80 [550] | 35 [240] | 20 | ||||||
304LN, 316LN S30453, S31653 |
75 [515] | 30 [205] | 35 | ||||||
N08367 t≤0.187 | 100 [690] | 45 [310] | 30 | ||||||
N08367 t>0.187 | 95 [655] | 45 [310] | 30 | ||||||
N08926 | 94 [650] | 45 [310] | 35 | ||||||
S31254 t≤0.187 | 100 [690] | 45 [310] | 35 | ||||||
S21254 t>0.187 | 95 [655] | 45 [310] | 35 | ||||||
S32654 | 120 [825] | 65 [450] | 40 |
Permissible Variations in Dimensions
Group |
Size, |
Permissible |
Permissible in WT, % |
PermisibleVariations in Cut Length, |
|
1 |
Up to 1/2(12.7), excl |
±0.005[0.13] |
±15 |
1/8[3] |
0 |
2 |
1/2 to 1 1/2(12.7 to 38.1 excl |
±0.005[0.13] |
±10 |
1/8[3] |
0 |
3 |
1 1/2 to 3 1/2(38.1 to 88.9 excl |
±0.010[0.25] |
±10 |
3/16[5] |
0 |
4 |
3 1/2 to 5 1/2(88.9 to 139.7 excl |
±0.015[0.38] |
±10 |
3/16[5] |
0 |
5 |
5 1/2 to 5 1/2(139.7 to 230.2 excl |
±0.030[0.76] |
±10 |
3/16[5] |
0 |
Reference Documents:
ASTM STANDARDS
ASTM A262 Practices for Detecting Susceptibility to Intergranular Attack in Austenitic Stainless Steels
ASTM A480 / A480 M Specification for General Requirements for Flat-Rolled Stainless and Heat-
Resisting Steel Plate, Sheet and Strip,
ASTM A941 Terminology Relating to Steel, Stainless Steel, Related Alloys, and Ferroalloys.
ASTM A1016/ A1016 M Specification for General Requirements for Ferritic Alloy Steel, Austenitic Alloy
Steels, and Stainless Steel Tubes.
ASTM E527 Practice for Numbering Metals and Alloys in the Unified Numbering System (UNS)
SAE J1086 Practice for Numbering Metals and Alloys (UNS)
Enter Your Message