316 Stainless Steel Quilted Grinding Hydraulic Cylinder Pipe
Contact Person : Richard SHEN
Phone Number : +86-13736164628
WhatsApp : +8613736164628
Minimum Order Quantity : | 1 tons | Price : | negotiable |
---|---|---|---|
Packaging Details : | Packing in bundles or as per clients' demand | Delivery Time : | 5-8 weeks days |
Payment Terms : | L/C, T/T | Supply Ability : | 5000tons per year |
Place of Origin: | China | Brand Name: | Torich |
---|---|---|---|
Certification: | IS09001 ISO14001 TS16949 | Model Number: | EN10305-1 |
Detail Information |
|||
Section Shape: | Round | Alloy Or Not: | Non-alloy |
---|---|---|---|
Technique: | Cold Drawn | Thickness: | 0.1 - 10 Mm |
Standard: | DIN,ASTM | Outer Diameter(round): | 4 - 50 Mm |
Application: | Hydraulic Pipe | Standard2: | DIN 2391 |
Special Pipe: | Seamless Tube | Product Name: | EN10305-1 DIN2391 4*0.9 4*0.6 4*1.1 Precision Steel Pipe Engine Fuel Injector |
High Light: | Precision Steel Pipe DIN2391,Engine Fuel Injector Precision Steel Pipe,Precision Hydraulic Seamless Pipe |
Product Description
EN10305-1 DIN2391 4*0.9 4*0.6 4*1.1 Precision Steel Pipe Engine Fuel Injector
The products are made of Baosteel steel billet raw materials and manufactured by German production technology.
The products meet the German DIN2391 and European EN10305-1/4 standards. Product features: high dimensional
accuracy, good internal and external surface finish, high-gloss surface, no oxide layer on the inner and outer walls of
the steel pipe after NBK normalizing heat treatment, good inner wall cleanliness, high pressure steel pipe, no
deformation after cold bending, no flaring, flattening Cracks can be processed for various complex deformations
and mechanical processing.
Precision Steel Pipe Engine Fuel Injector as per standard EN 10305 or DIN 2391
Chemical composition of EN 10305-1
Steel Grade | C | Si | Mn | P | S | Al | |
Steel name | Steel number | max | max | max | max | max | min |
E215 | 1.0212 | 0.10 | 0.05 | 0.70 | 0.025 | 0.025 | 0.025 |
E235 | 1.0308 | 0.17 | 0.35 | 1.20 | 0.025 | 0.025 | - |
E355 | 1.0580 | 0.22 | 0.55 | 1.60 | 0.025 | 0.025 | - |
Mechanical and techological properties of EN 10305-1
Mechanical properties at room temperature | |||||||||||||
Steel grade | Minimum values for the delivery condition | ||||||||||||
Steel name | steel nubmer | (+Cc) | (+LCc) | (+SR) | (+Ad) | (+N) NBK | |||||||
Rm Mpa | A % | Rm Mpa | A % | Rm Mpa | ReH Mpa | A % | Rm Mpa | A % | Rm Mpa | ReH Mpa | A % | ||
E215 | 1.0212 | 430 | 8 | 380 | 12 | 380 | 280 | 16 | 280 | 30 | 290-430 | 215 | 30 |
E235 | 1.0308 | 480 | 6 | 420 | 10 | 420 | 350 | 16 | 315 | 25 | 340-480 | 235 | 25 |
E355 | 1.0580 | 640 | 4 | 580 | 7 | 580 | 450f | 10 | 450 | 22 | 490-630 | 355 | 22 |